Halo-tellurite glass fiber with low OH content for 2-5μm mid-infrared nonlinear applications - Université de Rennes Accéder directement au contenu
Article Dans Une Revue Optics Express Année : 2013

Halo-tellurite glass fiber with low OH content for 2-5μm mid-infrared nonlinear applications

Résumé

We report the fabrication of new dehydrated halo-tellurite glass fibers with low OH content (1ppm in weight) and low OH-induced attenuation of 10dB/m in 3-4 μm region. It shows halo-tellurite glass fibers a promising candidate for nonlinear applications in 2-5μm region.

Domaines

Matériaux
Fichier principal
Vignette du fichier
Opt_Exp-Tellurite.pdf (1.82 Mo) Télécharger le fichier
Origine : Fichiers éditeurs autorisés sur une archive ouverte
Loading...

Dates et versions

hal-00858277 , version 1 (06-09-2013)

Identifiants

Citer

Feng Xian, Shi Jindan, Martha Segura, Nicolas M. White, Pradeesh Kannan, et al.. Halo-tellurite glass fiber with low OH content for 2-5μm mid-infrared nonlinear applications. Optics Express, 2013, 21 (16), pp.18949-18954. ⟨10.1364/OE.21.018949⟩. ⟨hal-00858277⟩
295 Consultations
609 Téléchargements

Altmetric

Partager

Gmail Facebook X LinkedIn More